| Availability: | |
|---|---|
| Quantity: | |
In a store, an automotive component faces three different loads: the steady weight of the stack above it, the short drop when a liner is set down a little too firmly, and months of quiet compression in between. Calling a liner "well cushioned" covers none of them. Specifying it means putting numbers to each, then choosing a density and thickness that satisfy all three at once.
The starting point is static stress—the part's weight divided by the contact area the liner actually provides. Against that value, a cushion curve gives the acceleration a material transmits at a given drop height. Read the curve for the selected EPE grade and the part's fragility level, and the required thickness follows: enough material to absorb the energy without bottoming out, but not so much that a shelf bay loses a layer of storage. This is why two parts of identical weight often need different liners.
Thickness is therefore a design variable, not a default. Sheet from half a millimetre to a hundred millimetres can be laminated to reach an exact build, letting one liner carry a deep recessed pocket beside a shallow pad. Too thin and impacts pass straight through to the part; too thick and the stack becomes unstable and the warehouse pays for air. The working target is a controlled deflection band under load—compressed enough to grip, far from the point where the foam collapses.
Density sets where that band sits. EPE is available from 18 to 45 kg/m³, with 20, 25, 30, and 40 as common production grades; Shore C hardness rises with it. Heavier castings sit on denser foam that resists taking a permanent set, while light trim pieces and sensor modules need the softer end so their own weight is enough to engage the cushion. Anti-static and flame-retardant grades cover the parts that ask for them without changing the calculation.
Long-term behaviour closes the specification. Closed-cell EPE returns over ninety percent of its thickness after compression—typically above ninety-five—and absorbs under a tenth of a percent water, so a liner stored through a humid season still seats the part the way it did on day one. Inspection criteria tied to permanent compression tell a store exactly when a liner is due for replacement rather than leaving it to guesswork.
Form follows the numbers: laminated pads bonded to PP hollow board for rigid support, die-cut or CNC-machined cavities, layer pads, and corner protectors—with hard edges kept away from painted and sealing faces. To specify yours, send the part weight, its contact footprint, the stack height, and the shortest drop worth protecting against. The reply should be a density, a thickness, and a measured transmitted-acceleration figure.