| Availability: | |
|---|---|
| Quantity: | |
Fit in an EPP liner is decided before the mould is cut. Its non polar surface resists adhesives and printing, and machining leaves a fuzzy edge, so a finished insert is rarely trimmed back to size. Shrinkage control is often listed as a drawback; it is really the specification to write down first. Everything downstream depends on it.
The tool drawing carries the dimensional decisions. The parting line sits away from faces that touch the component or seal against a lid. Every cavity gets a draft angle and generous radii so the part releases without dragging a wall. Wall sections stay as even as possible, since a thick corner cools and shrinks differently from a thin rib. Flat reference pads are moulded in for measurement.
Steam moulding adds its own variables. Bead expansion sets density, steam pressure and dwell set how well the beads fuse, and cooling sets the shape that leaves the tool. An EPP part keeps moving slightly after demoulding, so dimensions are agreed after a conditioning period, not straight off the machine. The tool is scaled from a measured shrinkage value for that geometry, not a generic percentage.
Fusion quality is checked as carefully as size. Poorly fused beads split along their boundaries under a drop, even when the insert looks sound and measures correctly. Sections are cut from a trial part, weighed for density, and pulled apart to inspect the bond. Load bearing columns and stack paths can be moulded at higher density while contact faces stay softer, with each zone drawn.
The crate interface closes the loop. The conditioned outer dimension must still clear the crate inner wall after washing, sit on the base ribs, and let the lid close without compressing the liner. Identification is moulded in as a raised field or colour code, because a sticker will not survive the cleaning agents a returnable loop uses. No shim should be needed at packing.
Verification follows the same timing. A first off tool part is measured after conditioning, fitted with a real component, then remeasured after vibration and a drop. Production lots record density, shrinkage, and fusion results against the mould revision. A tool change or a new bead lot triggers a fresh first article; a permanent dent, a bead boundary crack, or an out of band cavity means retirement.
To quote a liner that fits first time, send the part 3D data, faces that must not be touched, crate inner dimensions, stacked layers, drop and vibration requirements, temperature range, cleaning agents, target cycles, and annual volume. We return a tool layout showing parting line, draft, and wall sections, a shrinkage and density zone table, a conditioned first article report, and samples with drop and refit records.