One hardness across a whole insert forces a compromise. Soft enough to spare a painted surface and the cavity sags under load; firm enough to locate the part and that surface takes an imprint. EVA is useful here because its hardness can be set across a wide range, so the insert is specified as zones, not one block.
The variables are VA content, density, cross linking, and Shore A hardness. A resilient low density grade touches finished faces; a dense rigid grade holds datums and stacking paths with little permanent set. Zones are laminated, bonded, or moulded together, and each is colour marked so the zones cannot be swapped. The hardness map is agreed before any tool is cut.
Contact zones are the most sensitive. They are cut to sit on agreed non cosmetic faces, with rounded pocket entries and a fine, non abrasive skin. Where a lacquered, chromed, or polished part must be touched directly, a flocked or film faced EVA spreads the load and lowers friction, so vibration during a long haul does not polish a dull patch into the finish.
Locating zones do the opposite job. Denser EVA is used for datum pads, side walls, corner posts, and any rib that transfers a stacking load through the insert rather than through the component. The target is dimensional stability: after weeks under a loaded crate, the cavity still accepts the part with the same clearance it had on the day it was cut.
Under both sits a cushioning zone tuned to drop risk. Thickness and firmness set the travel before the part bottoms out, and a grade with a low compression set is chosen so the insert recovers between trips. Sample liners run a drop sequence, a repeat fit check, and a wash cycle, because a foam that performs once but creeps after cleaning is not acceptable.
Manufacture follows the volume and the zone layout. CNC cutting handles prototypes and hard grade blocks without a tool; hot pressing or moulding suits repeat orders and laminated constructions. Adhesives are selected against the cleaning agents in use, and bond lines are kept away from part contact faces. Every finished insert is checked for zone placement, edge burrs, and the clearance to the crate wall. Batch records link each hardness grade to its sheet lot.
To build the map, send the part drawing with weight, surfaces that must not be touched, drop and stacking requirements, cleaning agents, temperature range, and target cycles. We return a zone drawing with a stated hardness for each area, sample inserts, and a trial report covering fit, drop, wash, and repeat fit. The specification then lives on the drawing, not in a material datasheet.