Shallow tray cavities are a commodity; deep ones separate suppliers. The deeper the cavity, the further the heated sheet must stretch, and the thinner the walls become at exactly the places that carry load. Controlling that thinning is the difference between a deep tray that works and one that quietly fails in the rack.
The governing number is draw ratio: cavity depth against its opening width. Ratios beyond roughly one-to-one put serious demand on the material, because every millimetre of depth is bought by stretching the same area of plastic thinner. Above that line, process design matters more than sheet thickness.
Thinning follows geometry. The sheet sticks first where it lands, at the cavity rim, and stretches last into the deepest corner, so corners and floor transitions end up with a fraction of the starting gauge. A tray specified at three millimetres can measure under one at a sharp floor corner, which is where cracks start under load.
Three process tools fight the gradient. Zoned heating keeps the sheet hotter where it must stretch furthest and cooler where it must stay thick. A pre-billow blows the sheet into a dome before vacuum pulls it down, pre-stretching it evenly. A plug assist pushes matched tooling into the cavity, carrying material into the deep sections mechanically rather than leaving vacuum to do all the work.
Corner design is part of the answer as much as the machine. Radii in the draw direction let material flow around the corner instead of bridging across it, and a generous radius at the floor junction prevents the thin ring where most deep trays eventually split. Small radii look crisp on a drawing and fail on a pallet.
The applications that need this are the tall ones: housings nested two deep, tall battery modules, instruments standing vertically, and cavities deep enough that a part sits below the tray rim where side walls protect it. A deep tray also gains stacking value, because the part is captured rather than merely held.
Draft and release scale with depth. A deep cavity locks around the part as it cools, so wall taper and release texture are engineered from the start; pulling a part from an undersized deep cavity is where operators decide the tray is rubbish, regardless of what the drawing promised.
Verification is measured thickness, not appearance. Sign-off includes gauge readings at named points: floor centre, corner transition and rim, with a minimum thickness figure for each. Later batches are sampled against those numbers, so wall-thinning drift from a tired heater zone is caught before it reaches the parts.
Sheet selection closes the loop. Deep draws need a grade with high elongation at forming temperature and controlled memory, so the sheet that stretches into a tall corner relaxes back to shape rather than whitening and splitting. The sheet and the tool are specified together for that reason.
Describe the cavity depth, the part weight and the gauge you assume, and the response includes the achievable draw ratio and the thickness you can actually expect at the floor.